after reading this post awhile back, I knew I needed to order the green AEN dye. I really liked the color in that picture. I didnt remember what color green I had already, but obviously wasnt green AEN because my green is a good bit darker then that.

Well, I ordered some green AEN dye. Yep, its the same green dye I already had and neither are close to that picture. Maybe if you dunked the part in yellow after the green AEN it would get that bright of green.....

Just an FYI for anybody dye shopping and reading this post.