Sigh... Well, yeah, I can SEE the colors OK, I just can't distinguish between the darker ones very well. I've tried on 3 different monitors, 1 flat panel monitor and 2 different CRT monitors and although the colors vary a little, it's still nearly imposible to tell the darkest colors apart on any of my monitors, and I really doubt that the 2 browns, electric blue, and olive drab are all as close to black as the chart implies.
Can you honestly tell me that folks can distinguish between brown GL and brown BL on your chart?
It seems pretty unlikely, since those 2 color swatches are IDENTICAL, both with hex color values of #1A0D02. Are the 2 dyes also identical?
I see others have complained about the chart before on this board, so it must not just be me....
Steve
|