Acid for anodizing
Is automotive battery acid the same mixture (1/3 acid, 2/3 water) from all sources? The plating manual recommends getting it from NAPA auto stores for use in anodizing, but I have some from a different source. Does it matter as long as its automotive battery acid?
|