You can strip the chrome using muratic(hydrochloric) diluted 50% with water. Stainless can be polished to look nearly as good as chrome and will hold it's shine well. I think the chrome was used for scratch resistance on those pieces. It's your call on whether or not to re-chrome them. I wouldn't unless your going to be judged by real sticklers.
|