Sorry for the delay posting, I've been out of town working my real job. I finally remedied the spot problem on the marker by polishing it using black, brown and green compounds. The marker anodized fine with out spots after the polish job. Still not sure what the problem was but I have informed my son to please stay away from Timmy’s for now until we get a little more experience with various alloys.