Quote:
|
Originally Posted by scocklin
I’ve found that good results depend on a number of factors;
(snip)
2. Tight PH control especially with red dyes where I mantain a PH range between 5 & 6. (snip)
|
Thanks scocklin for the tips.
What do you use to adjust the dye pH?
I don't see anything about it in the Caswell anodizing manual (lcd_ano,pdf) and my dyes arent here yet....
If I knew what was used to adjust the pH I might be able to hunt some up this week.