Default removing chrome from brass

Hi Gus:
No, I dont reverse plate. It seems to attack the base metal and then I have to finish the part even more to remove the etching.
Usually you only have to remove chrome, activate the nickel, then either copper plate or nickel plate, then chrome.
Hope this helps.