View Single Post
  #4 (permalink)  
Old 07-08-2005, 03:08 PM
customandsound
Guest
 
Posts: n/a
Default

palm sanders are great .. but you need to get down and dirty with some greaseless or hand sanding to make it shine.... 80 is to harsh ... rebead it with #8 or 10 wet sand it then polishing it you should be ok from there .. but that auto wax is not good for what you are doing ... buy a started kit and you will love it