View Single Post
  #8 (permalink)  
Old 07-17-2005, 06:49 PM
pickleboy's Avatar
pickleboy pickleboy is offline
Metal Finishing Guru
 
Join Date: Feb 2005
Location: belleville michigan
Posts: 635
pickleboy is just really nicepickleboy is just really nicepickleboy is just really nicepickleboy is just really nice
Default

hey steve the trick on the chuck is to wrap it in duct tape. as for the bobs leaving lines it should work out on the next coumpound. and the glazing is just like the wheels, they need to be cleaned from time to time. i use a straight screwdriver blade(gently) or they will shred.
__________________
when in doubt polish it out/ why replace it when you can refinish it
G2 Polishing and Powdercoating
Reply With Quote