Build up of lead anodes
Has anyone tried casells instructions on page 11 of the manual on stoping the build up of lead anodes using the chrome tank. My anodes are used and they are causing problems with build up, I was wondering if I need to buy new plates and do the process on them are try to clean up my old ones. It gets old grinding the plates every time I have to fire up the chrome tank.
|