Quote:
|
Originally Posted by Popeye
You want to off-gas the parts at a higher temp and a longer time than you cure. 425 or 450 at 20 is fine, just cure at 375 or 400.
It's always a good idea not to touch any part once it's been cleaned.
IMHO
|
Well i cured at 400 for 20 minutes. And outgassed at 425 for 20 minutes.
As for masking stuff off, do you guys do it before it gets outgassed, or after? I found that my tape shrinks after being heated, so masking it before outgassing is pointless, as I would have to remask after as well, which of course requires the touching of the part.