You can blast them, hand sand them with 220grit sand paper, preheat and coat them. If he wants satin black just use a single coat of satin black, if you want to clear them use a satin clear or they will be glossy. Make sure you cure the satin black, it will stay glossy to it cools down to room temp after the cure.
|