I own and operate a powder coating shop, I will tell you if you get good with the hobby guns from any of the companys you described it will be hard to tell the difference from a part that was sprayed and coated with a pro gun. The only complaint I ever had is they are broken very easly, and the thickness varies more often since you really have to judge by eye how thick your applying it, with a pro gun you can dial that in.