Thread: Power Coating
View Single Post
  #1 (permalink)  
Old 02-14-2002, 02:47 AM
Rick M Rick M is offline
Newbie
 
Join Date: Feb 2002
Posts: 1
Rick M
Default Power Coating

I am using the power coat system to repaint some old erector set parts. I just got to try
out my new sprayer today very nice. Some of the pices came out different colors. I was using yellow couple of pices were real nice a
couple came out like under spray. I though I had covered them about the same. My question is is my heat possibly inconsient or did I over bake? Another question can you apply to much power an cause the paint to run in the baking process? I have never been very good at painting but I think power coating is my answer to a good paint job for me.
Thanks Amature Rick