Hey Netnut. It's tough to tell by just looking at the picture but I wonder if you have a condition called blooming. I'm not completely sure what causes it(something in the manufacturing process of the powder) but I've seen it in candies and clears. Basically the part developes an inconsistant almost blotchy haze. Almost looks like frost, but has no texture to it. Well if that's it, the only way to get rid of it is by reshooting the part.
|