one thing i have not heard mentioned is the importance of a good electrical contact. make sure your parts have a very good contact at the rectifier,buss bar and item to be plated. remember you are using low voltage and high amperage. just like a car battery. bad contact and your car won't start.bad contact and your part won't plate!