Default How dark is the olive drab? + zinc question.

Hi. I've purchaced the zinc plating kit and the yellow chromate as well. I have two questions. The zinc is plating ok, but some pieces come out nice and bright, and some (same item) come out like they were copy cad. I have added brightener and still no difference. Sometimes I will plate two identical items and one will be great while one has the copy cad kind of whitish look to it. Any ideas
I would like to redo some hardware on an older Jap motorcycle. Bolts, nuts, small brackets. At first glance They look black, but in the right light they are definitly dark green. Would your olive drab solution give a very dark, almost black finish on a fresh zinc plating? Thanks for your time.