Re: HELP! can't identify chemicals
The 'yellow' puzzles me. The dark mollasses one is the chrome.
For the blue ones, dip your fingers in , then rub them together gently. If they feel slippery, it's Flash Copper.
For the other blue, take a spoonful out and drop some baking soda into it. If it fizzes like crazy, it acid copper.
Copy ?. If that is yellow, then it's probably Copy Cad. Boy, the seller didn't do you any favors. I hope you 'stole' the kit from him.
|