Quote:
|
Originally Posted by tavo1765
2. 8x6x6 electric oven, I only use it when coating larger parts.
Now for my problem.
My smaller oven works excellent all the time. I place large items that use all its space and also fill it with a ton of smaller items, my temps range from 350-450f. All the parts cured in this small oven come out smooth like glass.
Now when starting up my larger oven it takes up to about 30hr to get to about 375f/ or 386 which is about 400f in my oven.
|
That's a typo (30 Hours) right? You meant 30 mins I hope. My 6x4x4 electric oven heats in about 20 mins, and the results are excellent. I almost always use the oven from cold start. Only because I'm a clutz and always burned myself trying to get things leaded into an already hot oven, never had a problem starting at room temp.
Your oven's curculation fan is operating properly I assume? Is this a new problem, or from day one?
Keith