Thread: Filling pits
View Single Post
  #5 (permalink)  
Old 08-25-2005, 08:06 PM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: Filling pits

You said it man, practice makes perfect but how much practice I wonder. YOur right I see why their is just a few of use doing the plating. I learn from watching others and then I try it my self, I wish I could watch you sometime and then I could see just what you do and how you do it. I am doing good at fillng, its just those little blisters that get me. THe only way I know that the part is going to come out right is just grind the pits out and hope that the part is not to thin.