Re: Glow in the Dark Additive Help HELP!!!
I used an empty 1 gallon ice cream container, put my clear coat in, then the holographic pigment, then used an electric kichen mixer (bought from the trift store Can$ 5.00) and mixed for about 5-8 minutes
Hope this helps
fr
|