Re: Glow in the Dark Additive Help HELP!!!
glow over black won't glow as good , it will glow but not as good as light colors
I have use it over red and blue and it still works nice.
ussing it over polish aluminum works, it will dull the finish a little but works nice.
I buy the glow additive and mix it with 1-1/2 Lb of clear powder
just add it and shake it.
BTW charge the powder and coat at a low light so you can see what you are doing and get an even coating , the biggest problem I've had with glow in the dark clear is that if you don't get a perfect even coat it will glow more in some spots .
|