Default

I could get a 1inch by 2foot section in about 30mins. I reguarly put polishing grease on the wheel. 1 quick hit against it every minute. It does take time to figure out what needs to be done. How thick do you have your wheels stacked together? If I was doing something that small I would have 3 6inch cotton sewn wheels put together to cover the whole workpiece that way you'll cover the whole part in one swipe.
__________________
This is my 85 Sport Coupe that I have nearly fixed up completly.
http://www.thirdgen.org/rides/rideimages/ACFmIX2CQ.JPG