I have done some pieces on bumpers like extensions I have posted the on this site now they were scratched deep and we used a tig to fill them in. If your plan is to use the pnp take time to practice
I cant stress this enough and remember that no plate will stick to chrome so the area you are working with will have to be stripped just the chrome not the nickel or copper underneath another way to fill theses scratches would be silver solder or Caswell’s plum-loy there are also some other products in the Caswell’s catalog that you might look at .
Practice makes perfect
Hope I’ve been able to help
Good luck