What I have done to get into smaller areas that I buff is to get 1", 1 1/2" and 2" buffs and double stack them on their mandrels. I use the spiral sewn either the plane or hard ones (yellow). You can also use a Dremel type felt buff and sand it down with 80 grit sandpaper to make it fit in the smaller areas.