Re: building a spray booth
I was going to vent it outside my shop using a flexible dryer duct and outlet, but i'm going to have to do some work on it because the 4" duct is not large enough to let the amount of air exit the booth. If you look at the picture above, I had to place duct tape around the outer edges of the filter because there was some air turbulance on the outer edges that was actually blowing backwards instead of sucking air through the filter. It does a decent job but I'm thinking now about closing off the exhaust on top and putting a port in the side and attaching my 5hp shop vac to it, I think that will do better. Anyhow, it's great not to have to clean stray powder off everything.
|