Re: What to replace sand with (blasting) ?
One thing I might add to Jim's post, by the way it is an excellent post.
When blasting steel with soda you don't have to prime it right away. The soda leaves a coating on the steel that will last up to 2 month before the rust starts to show and you have to prime it.