Ok.... I didn't raise the bath temp, but made sure parts were moved away atleast 3 inches from the anodes. What I did was split the anodes in 2 so I had 4 instead of 2. They were placed every 90 degrees around the tank. When we did this the result was more dark spots on the part. So then we took 2 of those anodes out and so we only had one anode split in 2 180 degrees apart around the tank. This didn't seem to help either. I just don't know what to do. I guess I will have to talk to technical support.\