Default Re: aluminium motorcycle wheels - pc'ing cause failure?

Just an idea for some. I've worked machine shop for years and dealt with aviation parts some of which were heat treated. If a heat treatment business can be found local give them a ring and check with them on the effects on aluminum. SS