View Single Post
  #4 (permalink)  
Old 09-26-2005, 12:44 PM
CaptainChauncy CaptainChauncy is offline
Amateur Metal Finisher
 
Join Date: Aug 2004
Posts: 68
CaptainChauncy is an unknown quantity at this point
Default Re: masking - how to get a fine line?

Here is a picture or some handle bars I did. I already returned the parts so I can not get a bettter picture but this should do. I used green high temp tape and just put it on very tight so it would not come loose. I usually use something flat to press the green tape down so it will be tighter.
Attached Thumbnails
masking-how-get-fine-line-resized-img_7175.jpg  