Questions about masking and how the powder stays on
My first question is about masking. Is it better to leave plugs, tape, etc on while baking or just take them off after coating. I read that taking them off off befre baking will leave a cleaner edge but is there any downside? Some stuff wont matter but on valve cover lettering and such I will want really clean edges. Removing them before baking also allows for cheap masks like regular tape, corks, etc.What are the advantages/disadvantages of each way?
Also I'm curious how the powder sticks to the piece after you have coated it and have taken the ground off to stick stuff in the oven. I mean it cant just fall of right? Do you have to be super careful not to touch or even bang the piece before its cured?
Got my oven, spray booth, and spraying rack tonight, gun, powder,etc should be here midweek. I cant wait to try it out.
Thanks
Adam
|