View Single Post
  #4 (permalink)  
Old 10-06-2005, 05:11 PM
PowderVisions PowderVisions is offline
Newbie
 
Join Date: Oct 2005
Location: Minnesota
Posts: 28
PowderVisions is on a distinguished road
Default Re: Hey another question! Powder Gun acting weird

I would also try testing the powder to see if it has moisture in it. To do this, take a handfull and sqeeze it hard together. It should fall apart fairly easily. If it stays balled tightly together, your powder will have to be fluidized in a dry hopper until it is acceptable. This type of thing happens in humid atmoshpheres. In dry atmospheres, the powder doesn't seem to want to stick to the part no matter what. In this case, you would take a wet mop and mop your floor to add some moisture into the room.