Sorry I haven't been on here in a REAL long time, I have been lurking from time to time

.
I was just curious though, how much powder does a normal frame need?
I plan on using my IR lamp and a couple of reflectors, any idea how long something like that might take to cure?
I have been sand blasting the frame with black oxide for what seems like the past month and no matter what I do, flash rust comes around when it site overnight. Can I use a fine grit(120?) sanding sponge to get rid of the flash and clean re clean the entire thing w/ acetone before spraying? anybody else have another suggestion?
Thanks for any help
This is my biggest job yet so wish me luck.