Re: Satin Chrome on Pot Metal
To achieve a satin finish after polishing simply use a scrubber wheel available through Caswell
on the surface of your part before your final plate. This is the process I use it works very well .
Quick break down
1 polish
2 flash copper
3 acid copper ( if using)
4 nickel
5 scrubber wheel (lightly)
6 final plate
remember to rince between steps and do water brake test