I seem to be having a problem and its gotta be user error

For right now I've been sanding using a sanding sponge but I can't seem to get away from scuffing the coating. I've also tried using a dremel, talk about a bad idea. It slips after grabbing the edges and the finish doesn't come out uniform unless you take your time and polish everything
Any ideas to speed up the process and keep it looking good? should I be using a small block with 220 sandpaper instead of the sponge? some of the lines I'm dealing with are 1/16" get to be a real pain to deal with.
thanks for any help