Tell me what am I doing wrong. My SP Degreaser doesn't seem to cope with even simple task. It is setup in a 5 gallon plastic bucket, mixed as per manual (1 bag per 2 gallons of water), heated to 134F. I did a simple test:
1. spray a large washer with WD-40
2. place in a shallow plate with water, water is repelled from the waser
3. soak in SP Degreaser for 15 minutes
4. rince with household hot water
5. this is where things are not as expected, place the washer in water and it IS STILL REPELLING, the washer even feels greasy.
Please advise on corrective action or an alternative degreaser available locally. Acetone is kind of expencive in 4-5 gallon quantity. Thanks.