Default Re: Titanium wire spring clips

Yes, I know others on here have stated that. After wondering why the Ti rack manufacturers SWEAR that you dont have to and a couple people on here SWEAR you do, I invested the time and money to experiment myself.

I was originally adding extra current to compensate for Ti racking also.....going by what I read on this forum. After you prime the rack, I wouldnt worry about adding extra current unless your running a small part on a large rack(going off memory and not my notes, i think this is the only time I noticed the rack making a difference).