Default Re: Keep getting blisters in flash copper plating...HELP

That Is Not Your Problem Your Problem Is Nickle Strike You Must Nickle Strike After You Zinc. Drip Dry. Always Dip Part Into Distilled Water Befor Going Into Another Bucket