i have a bucket of Caswell stripper made up that i have been using heavily for the last 2-3 months to strip various paintball marker parts and it works great for me. it is really hit or miss on timing. some ano's will come off in 1 minute some i have to leave in for 10+ to get some of the stubborn spots.

My only thing is my stripper solution is pretty much black at this point, im assuming due to the large amount of anno i have stripped from many parts most of them being black or very dark colors.