Alright, I just recently upgraded to 3/4hp with 12amps at 3450RPMS. I am stacking 4 8" wheels on the machine and can't even slow it down. I no longer have to heat the part up at all with a torch, the wheels get the part up to temp very easily. No more streaks, no more compound buildup, works flawlessly now.