Do not under any circumstances use the oven in your home for powder coating. Find an old one used and place it in your garage. Sandblasting the old paint off prior to powder coating works very well and gives the powder a good surface to adhere to.If you have a compressor already and find an oven then yes the kit is all you need. Plus ordering the color powder you wish to use. Yes it is simple just requires a little trial and error to develope techniques that get you the results you are after.