Thanks for the heads up, I hope that doesn't happen. If it does, it will be pretty easy to drill the rivets out and put in something else, since nothing overlaps the interior panels. Yeah, I'd like to see a pic or two if you get a chance.

Maybe I'd better add a couple of studs as stiffeners.