Default Re: Anodizing calculations (720 Rule)

When I first introduced to 720 Rule to this website in January 2004 it was a response to help in color consistancy. I am very impressed in how far the 720 Rule has progressed on this web site. I have not been able to visit or respond to forums on this website due to contract obligations with an employer, but that is now completed and I have been reading the forums again on Caswell and again I am impressed by the knowledge passed along. Please keep it going!
And just a side note on the firguring of rack size and the 720 Rule- Yes, you will need to figure in rack size only if you are doing eletrolytic color. Some of our rack designs have been over 1,000 ft2 alone per 30' load bar.