I would strongly advise not trying to put the tripoli on an abrasive nylon wheel. That would be pointless. I also would advise getting a tube of 80 grit greaseless compound or use all of the grits, MUCH better than hand sanding(especially for initial cut). I would stop at 800 grit wetsand and go to tripoli if you choose to handsand. Or you could use emery after say 240 or 320. Your choice. You have many options.