Re: brown spots after copy chroming
I have the 44gallon tanks the wheel chroming kit. I have use the zoop seal and i still have the brown spots. I have use turtle wax and also a mothers polish. As soon as i polish and just sprinkle a little water and leave it for a few secounds the brown spots appear. I am really in a bind with this. That only occurs with the copy chrome.
|