I have already finished sanding all the way up to 1500, I then buffed with brown then white it came out great except the small scrathes, so i decided to go for some help, after going through this forum i decided to try the emery with a 4" sisal wheel to try and get better results. I finshed all of the compounds and then took a look, for some reason it is dull it never happend when i used only brown/white but now its just not as polished looking as before. any help on this would help a ton thx's