Re: Oven using metal studs and aluminum
Steve,
Do you have an air inlet and a vent on the oven? When powder cures it smokes and stinks... it has to be vented!
IMHO
"Oven exhaust must be suitably sized to remove the gases that are a
natural by-product of the cure process."
Last edited by Popeye; 12-27-2005 at 04:42 PM.
|