I know this is not part of you question, but here is what I think would sure help on the video.
Where parts are milled out for letters, serial numbers, name brand. We need a good easy way to be able to mask this, maybe with some type of coating that can be applied then wiped off flush the the letters (that are below flush) will not anodize. I done one and it worked, tried another and it failed. This would be a big step for anodizers to customize some of our work, one more notch on the big commercial people.
Am I the only one who has an interest in this ?
Clint
|