Ok now I changed my setup from the drill and 4" wheel to a 3000 RPM car buffer with the arbor from Caswell and an 8" spiral buff and used the black compound the wheels where really looking good just some light compound marks washed wheel and dried and got new spiral wheel and went at it with the white bar now the shine lost it's depth so I tried the brown bar and no better is it possible that the wheel was to cold from just being washed it's only 24 outside where I washed it or is there something else any ideas