Re: New to Copy Chrome
First off, good luck with your kit. I started off with the small kit to learn things I could do and now I'm steadily growing. I do about the same thing your starting to do and have just opened a shop. The muratic acid and distilled water works the best for the pieces that you don't have to repair. I think you'll find that when you start running into pieces you have a blemish or scratch in you'll be wantting to get an acid copper kit also. I strctly do bike parts here and am waiting on delivery of the wheel kit so it will be easier to do inner primarys and larger parts. I do all the plating for the areas harley shop and other shops in the area so if you have any questions I'ld be glad to help. Enjoy your kit.
|